Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Seals Eastern Perflas® 9294 Perfluorinated Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Seals Eastern, Inc
Trade Name Perflas®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern Perflas® 9294 Perfluorinated Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Perfluoro rubber for aggressive chemical service. Perflas ® 9294 seals are made of a chemical resistant perfluorinated fluoroelastomer (FFKM). Perflas 9294 seals offer outstanding resistance to high temperatures (230°C/446°F) and all aggressive chemical environments. Perflas 9294 seals resist attack by nearly all chemical reagents, including organic and inorganic acids, alkalines, ketones, esters, alcohols, fuels and hot water. Information provided by Seals Eastern, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.13 g/cc
2.13 g/cc
ASTM D297, 15
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
Tensile Strength at Break 19.5 MPa
2830 psi
AVG; ASTM D412 Method A
16.58 MPa

@Time 252000 sec
2405 psi

@Time 70.0 hour
After Dry Heat Aging; ASTM D865
Tensile Strength, Yield 11.5 MPa
1670 psi
Stress at Elongation M100; ASTM D412 Method A
Elongation at Break 145 %
145 %
AVG; ASTM D412 Method A
240.7 %

@Time 252000 sec
240.7 %

@Time 70.0 hour
After Dry Heat Aging; ASTM D865
100% Modulus 0.0115 GPa
1.67 ksi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
ASTM D1329