Precision Polymer Engineering E80H Ethylene Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering E80H Ethylene Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sulphur cured, white Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration (FDA) to be in accordance with Code of Federal Regulations Title (CFR21), Section 177.2600.Applications: Material formulated for repeated use with aqueous foodstuffs intended for human consumption.
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
°IRHD; ASTM D1415
90
90
°IRHD, +10 change after 168 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 8.625 MPa
1251 psi
-25% change after 168 hours @ 125°C; ASTM D412
11.5 MPa
1670 psi
ASTM D412
Elongation at Break 131.25 %
131.25 %
-25% change after 168 hours @ 125°C; ASTM D412
175 %
175 %
ASTM D412
Compression Set 10 %
10 %
70 hours @ 100°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F