Tensile Strength, Yield 1070 MPa
155000 psi
Pacific Sintered Materials FN-253-T(HT) 4600 Powdered Metal
High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals.
Tensile Strength, Yield >= 1070 MPa

@Temperature 1025 °C,
Time 14400 sec
>= 155000 psi

@Temperature 1877 °F,
Time 4.00 hour
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar
Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect..
Tensile Strength, Yield 1070 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
Typical
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged
High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL..
Tensile Strength, Yield 1070 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
Typical
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4986
High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4986.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi..
Tensile Strength, Yield 1070 MPa
155000 psi
Hard
California Fine Wire Permanickel® K-300 Nickel Alloy
All values may vary dependent on specific design and usagePermanickel® is a registered trade name of the Inco family of products.Capabilities: WireRibbonInsulatedPlatedInformation provided by Calif..
Tensile Strength, Yield 1070 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 400 Thickness >80-100 mm
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea..
Tensile Strength, Yield 1070 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 400 Thickness 5 -
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea..
Tensile Strength, Yield 1070 MPa
155000 psi
Trans.
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate, Solution Treated Annealed
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Tensile Strength, Yield 1070 MPa

@Strain 0.200 %
155000 psi

@Strain 0.200 %
Bisalloy Steels BisPlate 400 Thickness 16-80 mm
A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea..