Material Notes:
High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-140HTAll information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 7.20 - 7.40 g/cc
0.260 - 0.267 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 39
39
Tensile Strength, Ultimate 1070 MPa
155000 psi
Tensile Strength, Yield 1070 MPa
155000 psi
Elongation at Break <= 0.50 %
<= 0.50 %
Modulus of Elasticity 152 GPa
22000 ksi
Flexural Strength 1590 MPa
230000 psi
Transverse Rupture
Charpy Impact, Unnotched 9.49 J
7.00 ft-lb