Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 1030 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 1030 MPa
>= 150000 psi
Parker Chomerics SPRING-LINE® Beryllium-Copper Gasket
Description: SPRING-LINE beryllium-copper gaskets combine high levels of EMI shielding effectiveness with spring-finger wiping and low closure force properties. The high performance qualities of ber..
Tensile Strength, Yield >= 1030 MPa
>= 150000 psi
Annealed and Aged
IBC Advanced Alloys FA230 Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Tensile Strength, Yield 1030 - 1250 MPa
149000 - 181000 psi
Materion Beryllium Copper Alloy 190 Strip; XHMS (TM08) Temper (UNS C17200)
Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 98%Stress Relaxation after 1000 hrs @ 200°C: 69%Formability Ratio, 90° Bend, R..
Tensile Strength, Yield 1030 - 1380 MPa
149000 - 200000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200)
Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 1030 - 1280 MPa
149000 - 186000 psi
Materion Beryllium Copper Alloy 25 Strip; 1/4HT (TH01) Temper (UNS C17200)
Treatment required for max strength: 2 hrs @ 315ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 70%Superficial Hardness: 30N 56-6..
Tensile Strength, Yield 1030 MPa
149000 psi
SSAB Tunnplat Domex® 034 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. General use of Domex® high strength steels offers a number of ..
Tensile Strength, Yield 1030 MPa
149000 psi
SSAB Tunnplat Domex® 044 BOR Oil quenched Boron Steel
Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron ..
Tensile Strength, Yield 1030 MPa
149000 psi
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction
The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati..
Tensile Strength, Yield 1030 MPa
149000 psi
Bar, Rod & Forgings
CMW® 73 Copper Alloy
CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w..
Tensile Strength, Yield 1030 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
Aged to ~ 40 HRC
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel
A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli..
Tensile Strength, Yield 1030 MPa

@Temperature 427 °C
150000 psi

@Temperature 800 °F
ATI Allvac® 718Plus™ Nickel Superalloy
Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the..
Tensile Strength, Yield 1030 MPa
150000 psi
Fully Hardened
ATI Wah Chang Tiadyne™ 3510
Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang
Copyright © lookpolymers.com All Rights Reserved