Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1030 - 1380 MPa | 149000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 1060 - 1380 MPa | 154000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
Tensile Strength, Yield | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy 25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
Tensile Strength, Yield | 1130 - 1380 MPa | 164000 - 200000 psi | |
Materion Beryllium Copper Alloy M25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |