Polymer Property : Tensile Strength, Yield = 1380 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1030 - 1380 MPa
149000 - 200000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 25 to 51 mm Thickness (UNS C17200)
Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 1060 - 1380 MPa
154000 - 200000 psi
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200)
Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In..
Tensile Strength, Yield 1130 - 1380 MPa
164000 - 200000 psi
Materion Beryllium Copper Alloy 25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17200)
Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i..
Tensile Strength, Yield 1130 - 1380 MPa
164000 - 200000 psi
Materion Beryllium Copper Alloy M25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17300)
Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i..