Multibase Multi-Flex® A 7727 HM Black TPE Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 7727 HM Black TPE Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM 792
Melt Flow 5.97 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.97 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
10 seconds; ASTM D2240
Tensile Strength, Yield 10.1 MPa
1460 psi
Elastic; ASTM D412
Elongation at Break 480 %
480 %
Elastic; ASTM D412
Flexural Modulus 0.265 GPa
38.4 ksi
1% Secant; ASTM D790
Tear Strength 66.6 kN/m
380 pli
ASTM D624
Thermal Properties Metric English Comments
Flame Spread 15 mm/min
0.60 in/min
FM VSS-302