Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.24 MPa | 180 psi | at 200%, post cured- 2 hours at 177°C |
Multibase SILASTIC® C7-4535 DICUP R Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.24 MPa | 180 psi | @ 50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 504 Perfluoroelastomer Greene Tweeds Chemraz® 504, a 65 Shore A hardness perfluoroelastomer, provides an extremely broad range of chemical resistance and is perfect for services with low pressures and/or low temperatur.. |
|||
Tensile Strength, Yield | 1.24 MPa | 180 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-235 PERKADOX PD-50S Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | >= 1.24 MPa | >= 180 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7240 Ethylene-Propylene Rubber Potable water service. Chloramine resistant.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.24 MPa | 180 psi | ASTM D412 |
Saint-Gobain COHRlastic® R10490 Medium Fluorosilicone Sponge Rubber Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R1.. |
|||
Tensile Strength, Yield | 1.24 MPa | 180 psi | ASTM D412 |
Teknor Apex MONPRENE® MP 1880 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 1.24 MPa | 180 psi | For 8% nominal density aluminum foam |
ERG Aerospace Duocel® Aluminum Metal Foam |
|||
Tensile Strength, Yield | 1.24 MPa | 179 psi | ASTM D638 |
Cheng Yu Plastic E2320 Flame Retardant PET, 20% Glass Fiber |
|||
Tensile Strength, Yield | 1.24 MPa | 180 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
PolyOne Synprene® RT-3605 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingInformation provided by PolyOne.. |