Seals Eastern 7240 Ethylene-Propylene Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Seals Eastern, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 7240 Ethylene-Propylene Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Potable water service. Chloramine resistant.Information provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 48
>= 48
ASTM D2240, Type A
52
52
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 6.16 MPa
>= 893 psi
ASTM D412 Method A
10.09 MPa
1463 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield 0.614 MPa
89.0 psi
AVG Stress at Elongation M25; ASTM D412 Method A
>= 0.779 MPa
>= 113 psi
Stress at Elongation M50; ASTM D412 Method A
0.958 MPa
139 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 1.24 MPa
>= 180 psi
Stress at Elongation M100; ASTM D412 Method A
1.70 MPa
246 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 206 %
>= 206 %
ASTM D412 Method A
322 %
322 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.00402 GPa
0.583 ksi
ASTM D412 Method A
Shear Modulus 0.00134 GPa
0.194 ksi
ASTM D412 Method A
Secant Modulus 0.00378 GPa
0.548 ksi
ASTM D412 Method A
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -51.1 °C
-60.0 °F
ASTM D1329
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 10