Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.590 MPa
85.6 psi
ASTM D412
Polymax® Maxelast® C4800 TPE, Transparent
Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applica..
Tensile Strength, Yield 0.590 MPa
85.6 psi
at 50% Extension (0.5 x 0.38 x 2 in bead)
Momentive Performance Materials Ultraglaze® 4400 Construction Sealant
High strength, two-part structural glazing system. Cure Method: Condensation. Tack-free time 3 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of ..