Polymax® Maxelast® C4800 TPE, Transparent

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Nagtong Polymax
Trade Name Maxelast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymax® Maxelast® C4800 TPE, Transparent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Excellent clarityOvermold adhesion to polypropyleneUltrasoft TPEs with gel-like propertiesSoft and cushioning comfortSuperior colorabilityPVC, silicone, and latex freeTypical Applications:ConsumerPackagingHealthcareElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd
Physical Properties Metric English Comments
Specific Gravity 0.822 g/cc
0.822 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Stress 0.0600 MPa

@Strain 100 %
8.70 psi

@Strain 100 %
ASTM D412
0.120 MPa

@Strain 300 %
17.4 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield 0.590 MPa
85.6 psi
ASTM D412
Elongation at Break 880 %
880 %
ASTM D412