Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 56.0 MPa | 8120 psi | ASTM D882 |
Westlake Mxsten CV CV77515-F Plastomer
(discontinued **) Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s.. |
|||
Film Tensile Strength at Break, MD | 56.0 MPa | 8120 psi | ISO 1184 |
SIDPEC EGYPTENE® HD 5301 FB HDPE Film Applications:Strong thin filmCarrier bagGrocery sacksFilm properties were measured on 15 micron film extruded at a blow up ratio of 5:1, 8D neck height.Information provided by Interchim s.r.l., offi.. |
|||
Film Tensile Strength at Break, MD | 56.0 MPa | 8120 psi | ASTM-D882 |
Westlake Mxsten CV77515 Polyethylene Plastomer Mxsten CV Plastomer CV77515 resin is a polyethylene plastomer designed for blown film extrusion and food packaging that contains 1,000 ppm slip and no antiblock additives. Films produced with this r.. |
|||
Film Tensile Strength at Break, MD | 56.0 MPa | 8120 psi | ASTM D882 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Film Tensile Strength at Break, MD | 56.0 MPa | 8120 psi | Calculated from mfr's report of 165 N/cm per ASTM D828 and the typical thickness |
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Film Tensile Strength at Break, MD | 56.0 MPa | 8120 psi | ASTM D882 |
NOVA Chemicals Sclair® 11C1 Octene LLDPE Film Resin
(discontinued **) Low gel, Good processability, Excellent mechanical propertiesApplications: Shrink filmAdditives: Process stabilizerFilm properties are typical of blown film extruded at a blowup ratio of 2.5:1, but .. |
|||
Film Tensile Strength at Break, MD | 56.0 MPa | 8120 psi | ISO 527-3 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |