Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 15.0 - 40.0 MPa | 2180 - 5800 psi | Average value: 27.1 MPa Grade Count:145 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Film Grade". Each property range of values reported is minimum a.. |
|||
Film Tensile Strength at Break, MD | 30.0 - 40.0 MPa | 4350 - 5800 psi | ISO 527-3 |
Borealis Borclear™ RB709CF Polypropylene Ethylene Copolymer Borclear™ RB709CF is a propylene -ethylene copolymer. This grade is suitable for the manufacturing of unoriented film on blown film lines. Applications: Borclear™ RB709CF is recommended for seal.. |