Polymer Property : Film Tensile Strength at Break, MD = 3900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is ..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
MD-TD Average; ASTM D882
DuPont Elvax® 3150 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
15 wt% Vinyl Acetate.General Elvax® information: Elvax® packaging grade resins include low seal temperatures for use in coextrusions or for packaging temperature sensitive materials, excellent dra..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
D638
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength m..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
Westlake EF606 Low Density Polyethylene
Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
Westlake EF706 Low Density Polyethylene
Westlake EF706 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
Formosa Plastics Formolene® L42022B Film (Butene Grade) LLDPE
Butene Copolymer (Barefoot)Applications: Blown and cast filmBlown and cast filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of p..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
Formosa Plastics Formolene® L42022E2 Film (Butene Grade) LLDPE
Butene Copolymer (Low slip and antiblock)Applications: Thin gauge blown filmThin gauge blown filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, cove..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil LD 124.MS General Purpose Clarity Film Resin
Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil LDPE LD 124.MS Low Density Polyethylene Resin
Product Description: LD 124.MS blown film resin offers an excellent balance of optical and strength properties for general purpose clear film applications. Availability: Latin America, North America..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil Escorene® LD 720.01 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
ExxonMobil Escorene® LD 720.62 Specialty Film Resin
Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D-882
Bapolene® 222F Polyethylene, Film Grade
Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/a..
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D882
DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..