Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 222F Polyethylene, Film Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 222F Polyethylene, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene LL222F is a general purpose LLDPE for blown film extrusion or cast film applications. This resin offers excellent tensile and toughness properties. It is available with and without slip/antiblock additives. This product meets FDA standards for food contact applications.Applications: Stretch wrap, produce bags, trash bags, drum and box liners.Film properties below are based on a thickness of 37.5 µm and blow-up ratio of 2:1.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Thickness 37.5 microns
1.48 mil
2:1 blow-up ratio
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.00 MPa
1310 psi
ASTM D882
Film Tensile Strength at Yield, TD 9.80 MPa
1420 psi
ASTM D882
Film Elongation at Break, MD 580 %
580 %
ASTM D-882
Film Elongation at Break, TD 800 %
800 %
ASTM D-882
Secant Modulus, MD 0.200 GPa
29.0 ksi
value @ 0.1 mm/mm-min Initial strain rate; ASTM D-882
Secant Modulus, TD 0.241 GPa
35.0 ksi
value @ 0.1 mm/mm-min Initial strain rate; ASTM D-882
Elmendorf Tear Strength, MD 6.70 g/micron
170 g/mil
ASTM D-1922
Elmendorf Tear Strength, TD 16.6 g/micron
422 g/mil
ASTM D-1922
Film Tensile Strength at Break, MD 26.9 MPa
3900 psi
ASTM D-882
Film Tensile Strength at Break, TD 20.7 MPa
3000 psi
ASTM D-882
Optical Properties Metric English Comments
Haze 20 %
20 %
ASTM D-1003
Gloss 38 %
38 %
ASTM D-2457
Processing Properties Metric English Comments
Melt Temperature 199 - 227 °C
390 - 441 °F
Descriptive Properties Value Comments
Process Film
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: