Polymer Property : Film Tensile Strength at Break, MD = 26100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 150 - 180 MPa
21800 - 26100 psi
ISO 527-3
Borealis BorPURE™ RB501BF Polypropylene Copolymer
BorPure™ RB501BF is a random copolymer. Applications: BorPure™ RB501BF has been developed especially for applications like: food packaging, over wrap film, label film, and shrink film. Additives..