Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 11.0 MPa
1600 psi
ASTM D882
Huntsman PE5082 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con..
Film Tensile Strength at Break, MD 11.0 - 78.5 MPa
1600 - 11400 psi
Average value: 23.6 MPa Grade Count:31
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and..