Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 11.0 MPa | 1600 psi | ASTM D882 |
Huntsman PE5082 Extrusion Coating Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings (sugar paper and laminations).FDA Notes: Con.. |
|||
Film Tensile Strength at Break, MD | 11.0 - 78.5 MPa | 1600 - 11400 psi | Average value: 23.6 MPa Grade Count:31 |
Overview of materials for Low Density Polyethylene (LDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Extrusion Grade". Each property range of values reported is minimum and.. |