Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, MD | 72.0 MPa | 10400 psi | ASTM D882 |
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 0.8 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng.. |
|||
Film Tensile Strength at Break, MD | 72.0 MPa | 10400 psi | ASTM D882 |
ExxonMobil Exceed™ 363C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and.. |
|||
Film Tensile Strength at Break, MD | 72.0 MPa | 10400 psi | Orientation not specified; ASTM D882 |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Film Tensile Strength at Break, MD | 72.0 MPa | 10400 psi | Orientation not specified; ASTM D882 |
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan.. |
|||
Film Tensile Strength at Break, MD | 72.0 MPa | 10400 psi | Orientation not specified; ASTM D882 |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
Film Tensile Strength at Break, MD | 72.0 MPa | 10400 psi | 2.5 BUR; ASTM D882 |
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica.. |
|||
Film Tensile Strength at Break, MD | 71.7 MPa | 10400 psi | 20 in/min, 2.0 in Jaw Separation; ExxonMobil Method |
ExxonMobil Label-Lyte™ 28LLG MET OPP Film Product Description: A clear, one-side metallized, one-side treated oriented polypropylene film. The metalized layer is designed to provide a bright metal appearance in surface print or laminated ap.. |
|||
Film Tensile Strength at Break, MD | 71.7 - 78.6 MPa | 10400 - 11400 psi | |
3M 6145 Kraft Light Duty Reinforced Water Activated Tape 3M™ Light Duty Reinforced Water Activated Tape 6145 is used for box sealing and other packaging applications. This product has a fiberglass reinforced paper backing and a high tack water-activated .. |
|||
Film Tensile Strength at Break, MD | 72.0 MPa | 10400 psi | ASTM D882 |
ExxonMobil Escorene® HDZ-128 MMW-HDPE Blown Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.Can be processed on high stalk, pocket extrusion or cast lines. Films made from HDZ-128 exhibit an excellent stiffness balance. High thermal stabi.. |