Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 72.0 MPa
10400 psi
ASTM D882
ExxonMobil Exceed™ 350D65 LDPE/Hexene Tough Premium Liner Film Resin, 0.8 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D65 resin have outstanding tensile, impact streng..
Film Tensile Strength at Break, MD 72.0 MPa
10400 psi
ASTM D882
ExxonMobil Exceed™ 363C32 LDPE/Hexene Premium Cast Stretch Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and..
Film Tensile Strength at Break, MD 72.0 MPa
10400 psi
Orientation not specified; ASTM D882
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas ..
Film Tensile Strength at Break, MD 72.0 MPa
10400 psi
Orientation not specified; ASTM D882
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Film Tensile Strength at Break, MD 72.0 MPa
10400 psi
Orientation not specified; ASTM D882
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL..
Film Tensile Strength at Break, MD 72.0 MPa
10400 psi
2.5 BUR; ASTM D882
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film
This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica..
Film Tensile Strength at Break, MD 72.0 MPa
10400 psi
ASTM D882
ExxonMobil Escorene® HDZ-128 MMW-HDPE Blown Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.Can be processed on high stalk, pocket extrusion or cast lines. Films made from HDZ-128 exhibit an excellent stiffness balance. High thermal stabi..