Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Wire/Cable Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.917 - 2.00 g/cc
0.0331 - 0.0723 lb/in³
Average value: 0.988 g/cc Grade Count:76
Water Absorption 0.0100 %
0.0100 %
Average value: 0.0100 % Grade Count:8
Moisture Absorption at Equilibrium 0.0100 %
0.0100 %
Average value: 0.0100 % Grade Count:8
Environmental Stress Crack Resistance 1.00 - 1000 hour
1.00 - 1000 hour
Average value: 211 hour Grade Count:39
>= 96.0 hour

@Temperature 50.0 - 50.0 °C
>= 96.0 hour

@Temperature 122 - 122 °F
Average value: 1150 hour Grade Count:4
Melt Flow 0.200 - 12.0 g/10 min
0.200 - 12.0 g/10 min
Average value: 1.39 g/10 min Grade Count:75
Mechanical Properties Metric English Comments
Hardness, Shore D 44.0 - 53.0
44.0 - 53.0
Average value: 47.7 Grade Count:17
Tensile Strength, Ultimate 9.00 - 25.0 MPa
1310 - 3630 psi
Average value: 13.0 MPa Grade Count:20
Tensile Strength, Yield 8.34 - 20.7 MPa
1210 - 3000 psi
Average value: 12.3 MPa Grade Count:53
Elongation at Break 50.0 - 900 %
50.0 - 900 %
Average value: 371 % Grade Count:72
Elongation at Yield 13.5 - 50.0 %
13.5 - 50.0 %
Average value: 30.0 % Grade Count:14
Modulus of Elasticity 0.200 - 0.300 GPa
29.0 - 43.5 ksi
Average value: 0.220 GPa Grade Count:7
Flexural Modulus 0.125 - 0.300 GPa
18.1 - 43.5 ksi
Average value: 0.208 GPa Grade Count:7
Secant Modulus 0.193 - 1.20 GPa
28.0 - 174 ksi
Average value: 0.545 GPa Grade Count:3
Tear Strength Test 13.7 - 115
13.7 - 115
Average value: 25.0 Grade Count:9
Tensile Set 5.00 - 360 %
5.00 - 360 %
Average value: 24.7 % Grade Count:17
Thermal Properties Metric English Comments
CTE, linear 180 - 230 µm/m-°C
100 - 128 µin/in-°F
Average value: 218 µm/m-°C Grade Count:8
Melting Point 104 - 200 °C
219 - 392 °F
Average value: 113 °C Grade Count:15
Maximum Service Temperature, Air 200 °C
392 °F
Average value: 200 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 41.0 - 45.0 °C
106 - 113 °F
Average value: 42.6 °C Grade Count:5
Vicat Softening Point 87.8 - 93.9 °C
190 - 201 °F
Average value: 90.3 °C Grade Count:5
Brittleness Temperature -76.0 - -67.0 °C
-105 - -88.6 °F
Average value: -74.1 °C Grade Count:12
Flammability, UL94 HB - V-2
HB - V-2
Grade Count:10
Oxygen Index 17.0 - 24.8 %
17.0 - 24.8 %
Average value: 19.2 % Grade Count:7
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+6 - 1.00e+18 ohm-cm
1.00e+6 - 1.00e+18 ohm-cm
Average value: 3.44e+16 ohm-cm Grade Count:35
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Average value: 1.00e+14 ohm Grade Count:5
Dielectric Constant 2.03 - 2.70
2.03 - 2.70
Average value: 2.35 Grade Count:74
Dielectric Strength 2.17 - 49.6 kV/mm
55.0 - 1260 kV/in
Average value: 31.3 kV/mm Grade Count:58
Dissipation Factor 0.0000100 - 0.00700
0.0000100 - 0.00700
Average value: 0.000783 Grade Count:69
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:8
Processing Properties Metric English Comments
Processing Temperature 80.0 - 240 °C
176 - 464 °F
Average value: 150 °C Grade Count:6
Die Temperature 141 - 185 °C
285 - 365 °F
Average value: 174 °C Grade Count:10
Melt Temperature 120 - 230 °C
248 - 446 °F
Average value: 162 °C Grade Count:13
Head Temperature 140 - 185 °C
284 - 365 °F
Average value: 174 °C Grade Count:10