Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 22.0 MPa | 3190 psi | ASTM D882 |
NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin.. |
|||
Film Tensile Strength at Yield, MD | 22.0 MPa | 3190 psi | ASTM D 882 |
NOVA Chemicals Sclair® 17A Butene HDPE Film Resin 17A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Film Tensile Strength at Yield, MD | 22.0 MPa | 3190 psi | ISO 527-3 |
Total PPH 6088 Polypropylene Homopolymer, Cast Film Polypropylene PPH 6088 is a homopolymer polypropylene with a Melt Flow index of 9 g/10 min for the cast extrusion of film with excellent optical properties and good sterilizability.Polypropylene PPH.. |