NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Copolymer Film Grade
Manufacturer NOVA Chemicals
Trade Name Novapol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Novapol® HF-Y450-A Hexene HDPE Film Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Film Properties. Features: High strength and stiffness, excellent drawdown, used in blends with LDPE/LLDPE for improved film stiffness.Applications: Grease barrier, lamination films, blending resin, deli bags.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D792
Thickness 25.4 microns
1.00 mil
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 22.0 MPa
3190 psi
ASTM D882
Film Tensile Strength at Yield, TD 24.0 MPa
3480 psi
ASTM D882
Film Elongation at Break, MD 529 %
529 %
ASTM D882
Film Elongation at Break, TD 892 %
892 %
ASTM D882
Secant Modulus, MD 0.638 GPa
92.5 ksi
ASTM D882
Secant Modulus, TD 0.769 GPa
112 ksi
ASTM D882
Elmendorf Tear Strength, MD 0.500 g/micron
12.7 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 18.7 g/micron
475 g/mil
ASTM D1922
Dart Drop 2.70 g/micron
68.6 g/mil
F50, ASTM D1709/A
Film Tensile Strength at Break, MD 35.0 MPa
5080 psi
ASTM D882
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882