Polymer Property : Film Tensile Strength at Yield, MD = 26.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 26.2 MPa
3800 psi
ASTM D882
LyondellBasell Alathon® L5845 High Density Polyethylene
ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg..
Film Tensile Strength at Yield, MD 26.2 MPa
3800 psi
ASTM D882
LyondellBasell Alathon® L5005 High Density Polyethylene
ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi..
Film Tensile Strength at Yield, MD 26.2 MPa
3800 psi
ASTM D 882 A
Total 6410 HDPE Film Resin
Unique combination of high stiffness and clarity; Good moisture barrier properties; Good processability; Good compatibility with LDPE and LLDPEApplications: paper overwrap, cup overwrap, plate overw..
Film Tensile Strength at Yield, MD 26.2 MPa
3800 psi
ASTM D882, A 20 in/min
Total HDPE 6420 High Density Polyethylene, Film Resin
Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with..
Film Tensile Strength at Yield, MD 26.2 MPa
3800 psi
ASTM D882
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.Benefits. 4170 forms tough films with high dart imp..