Polymer Property : Film Tensile Strength at Yield, MD = 17.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 9.00 - 17.0 MPa
1310 - 2470 psi
Average value: 11.1 MPa Grade Count:48
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Butene, Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Butene, Film". Each property range of values reported is minimum..
Film Tensile Strength at Yield, MD 7.40 - 17.0 MPa
1070 - 2470 psi
Average value: 11.0 MPa Grade Count:48
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..
Film Tensile Strength at Yield, MD 15.0 - 17.0 MPa
2180 - 2470 psi
Average value: 15.9 MPa Grade Count:16
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..