Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D882 |
NOVA Chemicals Novapol® TD-9055-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of cast film extruded at 280°C.Information provided by NOVA Chemicals.. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-0338-E Hexene LMDPE Film Resin Excellent stiffness and glossApplications: Diaper back sheet, BlendingAdditives: High temperature AOFilm properties are typical of film extruded at 280°C.Information provided by NOVA Chemicals. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D 882 |
NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y534-IP Hexene LLDPE Film Resin Film Properties. Features: Excellent stiffness, excellent puncture, high strength and toughness.Applications: Industrial packaging, overwrap, narrow die gap extrusion.Data provided by the manufactu.. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | 2 in per min; ASTM D882 |
Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin
(discontinued **) Low Density, Linear Polyethylene Film ResinCustomer Benefits: This unique broad molecular weight distribution resin has a wide processing window and produces film with an excellent combination of to.. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PE 1304
(discontinued **) PRE-ELEC PE 1304 is a conductive thermoplastic compound based on a blend of PE-LD/PE-LLD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivi.. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D882 |
ExxonMobil Escorene® LD-708 EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 15.5% vinyl acetate copolymer film resin. Film made from LD-708 exhibits good impact strength and superior heat sealability.Applications: Primal .. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D882 |
NOVA Chemicals Sclair® 14A Butene MDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness, broad MW distribution.Applications: Co-extrusion, blending.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 15.0 - 17.0 MPa | 2180 - 2470 psi | Average value: 15.9 MPa Grade Count:16 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and.. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D882 |
NOVA Chemicals Sclair® 13J7 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, high clarity.Applications: Film.Data provided by the manufacturer. |
|||
Film Tensile Strength at Yield, MD | 15.0 MPa | 2180 psi | ASTM D882 |
NOVA Chemicals Sclair® 14J1 Octene LMDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, good clarity, high strength and toughness.Applications: Produce film.Data provided by the manufacturer. |