Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, MD | 11.3 MPa | 1640 psi | ASTM D882 |
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 3 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b.. |
|||
Film Tensile Strength at Yield, MD | 11.3 MPa | 1640 psi | |
Dow Elite® 5400 Linear Low Density Polyethylene 5400 enhanced polyethylene resin is a copolymer produced via INSITE technology from Dow Plastics. It offers extremely high impact resistance, combined with excellent tear, tensile, and optical prop.. |