Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 655 MPa @Strain 0.200 %, Thickness 12.7 - 25.4 mm |
>= 95000 psi @Strain 0.200 %, Thickness 0.500 - 1.00 in |
ASTM E-8 |
H.C. Starck 3403 Molybdenum Alloy APT-3 TZM, Arc-Cast Plate Arc-Cast Plate 3403Description of Product: This specification covers rolled plate of carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) produced from sheet bar consolidated .. |
|||
Tensile Strength, Yield | >= 655 MPa @Strain 0.200 %, Thickness <=0.0254 mm |
>= 95000 psi @Strain 0.200 %, Thickness <=0.00100 in |
ASTM E-345 |
H.C. Starck F-21-5 Pure Molybdenum, Foil F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli.. |
|||
Tensile Strength, Yield | >= 655 MPa @Strain 0.200 %, Thickness 0.0254 - 0.0508 mm |
>= 95000 psi @Strain 0.200 %, Thickness 0.00100 - 0.00200 in |
ASTM E-345 |
H.C. Starck F-21-5 Pure Molybdenum, Foil F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli.. |
|||
Tensile Strength, Yield | >= 655 MPa @Strain 0.200 %, Thickness 0.0508 - 0.0762 mm |
>= 95000 psi @Strain 0.200 %, Thickness 0.00200 - 0.00300 in |
ASTM E-345 |
H.C. Starck F-21-5 Pure Molybdenum, Foil F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli.. |
|||
Tensile Strength, Yield | >= 655 MPa @Strain 0.200 %, Thickness 0.0762 - 0.124 mm |
>= 95000 psi @Strain 0.200 %, Thickness 0.00300 - 0.00490 in |
ASTM E-345 |
H.C. Starck F-21-5 Pure Molybdenum, Foil F-21-5Description of Product: Rolled molybdenum foil from 0.001 inches through 0.0049 inches thick produced from pressed and sintered powder metallurgy sheet bar.Structure: All foil will be suppli.. |
|||
Tensile Strength, Yield | >= 655 MPa @Diameter 22.2 - 28.57 mm, Strain 0.200 % |
>= 95000 psi @Diameter 0.875 - 1.125 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Molybdenum Alloy PBT, Bar Powder Metallurgy BarDescription of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurg.. |
|||
Tensile Strength, Yield | >= 655 MPa @Diameter 22.2 - 28.57 mm, Strain 0.200 % |
>= 95000 psi @Diameter 0.875 - 1.125 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought bar produced from ingots consolidated by the H.C. Starck consuma.. |
|||
Tensile Strength, Yield | 655 - 862 MPa @Strain 0.200 %, Thickness <=25.4 mm |
95000 - 125000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bar |
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan.. |
|||
Tensile Strength, Yield | 655 MPa @Thickness 25.4 mm |
95000 psi @Thickness 1.00 in |
Longitudinal Direction |
Alcoa 7055-T7751 Aluminum Plate Alcoa introduced alloy 7055 in the -T7751 temper for plate and the -T77511 for extrusions in 1991. This alloy was developed for use in compression-dominated structures (such as upper wing structures.. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |
|||
Tensile Strength, Yield | 655 MPa @Strain 0.200 % |
95000 psi @Strain 0.200 % |
|
Crucible Steel 431 Chromium Steel Crucible 431 is a nickel bearing chromium steel which can be treated to exceptionally high physical properties. In the heat treated conditions, its corrosion resistance is superior to similar marten.. |