Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 655 - 862 MPa @Strain 0.200 %, Thickness <=25.4 mm |
95000 - 125000 psi @Strain 0.200 %, Thickness <=1.00 in |
Cold Drawn Bar |
Schmolz + Bickenbach LeanDupâ„¢ 35N Stainless Steel Bar Description: LeanDupâ„¢ 35N also known as (Uranus 35 N) is a dual phase austentic-ferritic stainless steel that has the ability to become as important as 316L. It offers better corrosion resistan.. |