Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 552 MPa @Thickness 1.57 mm |
80000 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP555 Carbon Fiber
(discontinued **) Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane m.. |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 %, Thickness 4.762 - 12.7 mm |
>= 80000 psi @Strain 0.200 %, Thickness 0.1875 - 0.500 in |
ASTM E-8 |
H.C. Starck 3203 Pure Molybdenum APL, Arc-Cast, Low Carbon Plate Arc-Cast Plate 3203 Low CarbonDescription of Product: This specification covers rolled plate of carbon-deoxidized molybdenum produced from ingots consolidated by the H.C. Starck consumable electrod.. |
|||
Tensile Strength, Yield | >= 552 MPa @Diameter 47.63 - 73.03 mm, Strain 0.200 % |
>= 80000 psi @Diameter 1.875 - 2.875 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Molybdenum Alloy PBT, Bar Powder Metallurgy BarDescription of Product: This specification covers molybdenum alloy (Molybdenum + 0.5% titanium + 0.1% zirconium) wrought bar produced from pressed and sintered powder metallurg.. |
|||
Tensile Strength, Yield | >= 552 MPa @Diameter 47.63 - 73.03 mm, Strain 0.200 % |
>= 80000 psi @Diameter 1.875 - 2.875 in, Strain 0.200 % |
ASTM E-8 |
H.C. Starck Molybdenum Alloy TZM ABT, Arc-Cast Bar Description of Product: This specification covers carbon-deoxidized TZM alloy (molybdenum + 0.5% titanium + 0.08% zirconium) wrought bar produced from ingots consolidated by the H.C. Starck consuma.. |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 %, Thickness 1.52 - 2.54 mm |
>= 80000 psi @Strain 0.200 %, Thickness 0.0600 - 0.100 in |
ASTM E-8 |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 %, Thickness 2.54 - 4.75 mm |
>= 80000 psi @Strain 0.200 %, Thickness 0.100 - 0.187 in |
ASTM E-8 |
H.C. Starck Pure Molybdenum, Sheet Premium Grade PS-100-2 Description of Product: Rolled molybdenum sheet produced from pressed and sintered powder metallurgy sheet bar.Structure: Sheet will be supplied in a stress-relieved condition unless otherwise req.. |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 %, Thickness 1.52 - 2.54 mm |
>= 80000 psi @Strain 0.200 %, Thickness 0.0600 - 0.100 in |
ASTM E-8 |
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect.. |
|||
Tensile Strength, Yield | >= 552 MPa @Strain 0.200 %, Thickness 2.54 - 4.75 mm |
>= 80000 psi @Strain 0.200 %, Thickness 0.100 - 0.187 in |
ASTM E-8 |
H.C. Starck 3202 Pure Molybdenum ASL, Arc-Cast, Low Carbon Sheet Arc-Cast Sheet 3202 Low CarbonDescription of Product: This specification covers rolled sheet of carbon-deoxidized molybdenum produced from sheet bar consolidated by the H.C. Starck consumable elect.. |