Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 550 MPa @Strain 0.200 %, Temperature -196 °C |
79800 psi @Strain 0.200 %, Temperature -321 °F |
EN min.; EN 10002-5 |
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | >= 550 MPa @Strain 0.200 % |
>= 79800 psi @Strain 0.200 % |
|
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Tensile Strength, Yield | >= 550 MPa @Strain 0.200 % |
>= 79800 psi @Strain 0.200 % |
|
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
Tensile Strength, Yield | >= 550 MPa @Strain 0.200 %, Temperature 350 °C |
>= 79800 psi @Strain 0.200 %, Temperature 662 °F |
|
ThyssenKrupp N-A-XTRA® 700 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | >= 550 MPa @Thickness 65.0 mm |
>= 79800 psi @Thickness 2.56 in |
|
ThyssenKrupp N-A-XTRA® M 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |