Polymer Property : Tensile Strength, Yield = 550 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 550 MPa

@Strain 0.200 %,
Temperature -196 °C
79800 psi

@Strain 0.200 %,
Temperature -321 °F
EN min.; EN 10002-5
Outokumpu 4311 Cr-Ni Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield >= 550 MPa

@Strain 0.200 %
>= 79800 psi

@Strain 0.200 %
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re..
Tensile Strength, Yield >= 550 MPa

@Strain 0.200 %
>= 79800 psi

@Strain 0.200 %
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40
Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red..
Tensile Strength, Yield >= 550 MPa

@Strain 0.200 %,
Temperature 350 °C
>= 79800 psi

@Strain 0.200 %,
Temperature 662 °F
ThyssenKrupp N-A-XTRA® 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield >= 550 MPa

@Thickness 65.0 mm
>= 79800 psi

@Thickness 2.56 in
ThyssenKrupp N-A-XTRA® M 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..