Outokumpu 4313 Martensitic Stainless Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel
Manufacturer Outokumpu
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Outokumpu 4313 Martensitic Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 850 MPa
123000 psi
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
Tensile Strength, Yield 650 MPa

@Strain 0.200 %
94300 psi

@Strain 0.200 %
EN min.,RT; EN 10002-1
700 MPa

@Strain 0.200 %
102000 psi

@Strain 0.200 %
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
770 MPa

@Strain 1.00 %
112000 psi

@Strain 1.00 %
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
530 MPa

@Strain 0.200 %,
Temperature 400 °C
76900 psi

@Strain 0.200 %,
Temperature 752 °F
EN min.; EN 10002-5
560 MPa

@Strain 0.200 %,
Temperature 200 °C
81200 psi

@Strain 0.200 %,
Temperature 392 °F
EN min.; EN 10002-5
590 MPa

@Strain 0.200 %,
Temperature 100 °C
85600 psi

@Strain 0.200 %,
Temperature 212 °F
EN min.; EN 10002-5
Elongation at Break 20 %
20 %
Outokumpu Typical, Quenched & Tempered Hot Rolled Plate (Quarto); EN 10002-1
Component Elements Properties Metric English Comments
Carbon, C 0.050 %
0.050 %
Chromium, Cr 13 %
13 %
Iron, Fe 82.45 %
82.45 %
Molybdenum, Mo 0.50 %
0.50 %
Nickel, Ni 4.0 %
4.0 %