Mechanical Properties Metric English Comments
Tensile Strength, Yield 410 MPa

@Strain 1.00 %
59500 psi

@Strain 1.00 %
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1
Outokumpu 253MA® High Temperature Austenitic Stainless Steel
Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be..
Tensile Strength, Yield 410 MPa

@Temperature 316 °C
59500 psi

@Temperature 600 °F
International Mold Steel DH21 Die Cast & Forging Steel
DH21 is for aluminum die cast dies.Information provided by International Mold Steel
Tensile Strength, Yield >= 410 MPa

@Strain 0.200 %,
Temperature 400 °C
>= 59500 psi

@Strain 0.200 %,
Temperature 752 °F
ThyssenKrupp N-A-XTRA® 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Tensile Strength, Yield 410 MPa

@Temperature 24.0 °C
59500 psi

@Temperature 75.2 °F
Dry
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel
Tensile Strength, Yield 410 MPa

@Temperature 23.0 °C
59500 psi

@Temperature 73.4 °F
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26T/50%/7581 Glass Fabric
300 gsmInformation provided by HexCel
Tensile Strength, Yield 410 MPa

@Strain 0.200 %,
Thickness 15.0 - 38.1 mm
59500 psi

@Strain 0.200 %,
Thickness 0.591 - 1.50 in
Typical Strength
Constellium Alumold® 400 Aluminum
The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds..
Tensile Strength, Yield >= 410 MPa

@Strain 0.200 %,
Thickness 100 - 120 mm
>= 59500 psi

@Strain 0.200 %,
Thickness 3.94 - 4.72 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..