Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 410 MPa @Strain 1.00 % |
59500 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 410 MPa @Temperature 316 °C |
59500 psi @Temperature 600 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
Tensile Strength, Yield | >= 410 MPa @Strain 0.200 %, Temperature 400 °C |
>= 59500 psi @Strain 0.200 %, Temperature 752 °F |
|
ThyssenKrupp N-A-XTRA® 550 Structural Steel This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng.. |
|||
Tensile Strength, Yield | 410 MPa @Temperature 24.0 °C |
59500 psi @Temperature 75.2 °F |
Dry |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |
|||
Tensile Strength, Yield | 410 MPa @Temperature 23.0 °C |
59500 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26T/50%/7581 Glass Fabric 300 gsmInformation provided by HexCel |
|||
Tensile Strength, Yield | 410 MPa @Strain 0.200 %, Thickness 15.0 - 38.1 mm |
59500 psi @Strain 0.200 %, Thickness 0.591 - 1.50 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | >= 410 MPa @Strain 0.200 %, Thickness 100 - 120 mm |
>= 59500 psi @Strain 0.200 %, Thickness 3.94 - 4.72 in |
|
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |