Polymer Property : Tensile Strength, Yield = 54000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 303 - 372 MPa

@Strain 0.200 %,
Thickness 0.508 - 1.52 mm
43900 - 54000 psi

@Strain 0.200 %,
Thickness 0.0200 - 0.0600 in
ATI Allegheny Ludlum 430 Ferritic Stainless Steel
Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily..