Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 303 - 372 MPa @Strain 0.200 %, Thickness 0.508 - 1.52 mm |
43900 - 54000 psi @Strain 0.200 %, Thickness 0.0200 - 0.0600 in |
|
ATI Allegheny Ludlum 430 Ferritic Stainless Steel Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.. |