Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 50.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 50.0 MPa

@Temperature 300 °C
>= 7250 psi

@Temperature 572 °F
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Information provided by PEAK Werkstoff GmbH
Tensile Strength, Yield 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
50%RH; ASTM D638
DuPont Performance Polymers Zytel® 7304 NC010 Nylon 6  (Unverified Data**)
Zytel® 7304 NC010 is a medium viscosity, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
90º, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
1947 - 38% resin weight with M46J 52.5% fiber volumeInformation provided by HexCel
Tensile Strength, Yield 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 7301 NC010 Nylon 6  (Unverified Data**)
Zytel® 7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications.Information provided by DuPont Performance Polymers
Tensile Strength, Yield 50.0 MPa

@Thickness 3.20 mm
7250 psi

@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Bhansali Engineering Abstron KU602L ABS Heat Resistant
High rigidityInformation provided by Bhansali
Tensile Strength, Yield 50.0 MPa

@Thickness 3.20 mm
7250 psi

@Thickness 0.126 in
Type I, 50 mm/min; ASTM D638
Bhansali Engineering Abstron KU602L ABS Heat Resistant
High rigidityInformation provided by Bhansali
Tensile Strength, Yield 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66  (Unverified Data**)
Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit..
Tensile Strength, Yield 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FG7301 NC010 Nylon 6  (Unverified Data**)
Zytel® FG7301 NC010 is a general purpose, unlubricated polyamide 6 resin for extrusion applications. It has been developed for consideration into applications such as parts for the food industry.In..
Tensile Strength, Yield 50.0 MPa

@Temperature 23.0 °C
7250 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610  (Unverified Data**)
Zytel® RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredient by weight. It is an unreinforced, heat stabilized, lubricated black grad..