Polymer Property : Tensile Strength, Yield = 497 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 497 MPa

@Temperature 23.9 °C
72100 psi

@Temperature 75.0 °F
0° Direction, Wet (2hr water boil); ASTM D638 Type 1
Park Electrochemical Nelcote® P-600 Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160..
Tensile Strength, Yield >= 497 MPa

@Strain 0.200 %,
Thickness 76.2 - 127 mm
>= 72100 psi

@Strain 0.200 %,
Thickness 3.00 - 5.00 in
Tempers T651 / T652
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..