Material Notes:
Nelcote® P-600 is a general purpose 190°F curing polyester system widely accepted as a cost-effective alternative to wet lay-up processingKey Features and Benefits:Meets MIL-R-7575 requirements160°F max service temperatureGood electrical propertiesLow cure temp (190°F) for easy processingApplications/Qualifications:Aircraft window framesIndustrial PartsAutomotive applicationsInformation provided by Park Electrochemical Corp.
Physical Properties Metric English Comments
Volatiles <= 2.0 %

@Temperature 135 °C
<= 2.0 %

@Temperature 275 °F
8 min
Water Absorption 0.38 %
0.38 %
ASTM D570 proc. 7.5
Mechanical Properties Metric English Comments
Tensile Strength, Yield 497 MPa

@Temperature 23.9 °C
72100 psi

@Temperature 75.0 °F
0° Direction, Wet (2hr water boil); ASTM D638 Type 1
514 MPa

@Temperature 23.9 °C
74500 psi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Tensile Modulus 23.4 GPa

@Temperature 23.9 °C
3400 ksi

@Temperature 75.0 °F
0° Direction, Wet (2hr water boil); ASTM D638 Type 1
26.2 GPa

@Temperature 23.9 °C
3800 ksi

@Temperature 75.0 °F
0° Direction, Dry; ASTM D638 Type 1
Flexural Strength 596 MPa

@Temperature 23.9 °C
86400 psi

@Temperature 75.0 °F
Wet (2hr water boil); ASTM D790
766.0 MPa

@Temperature 23.9 °C
111100 psi

@Temperature 75.0 °F
Dry; ASTM D790
Flexural Modulus 19.3 GPa

@Temperature 23.9 °C
2800 ksi

@Temperature 75.0 °F
Wet (2hr water boil); ASTM D790
23.4 GPa

@Temperature 23.9 °C
3400 ksi

@Temperature 75.0 °F
Dry; ASTM D790
Compressive Strength 450 MPa

@Temperature 23.9 °C
65200 psi

@Temperature 75.0 °F
Wet (2hr water boil); ASTM D695
527 MPa

@Temperature 23.9 °C
76400 psi

@Temperature 75.0 °F
Dry; ASTM D695
Electrical Properties Metric English Comments
Dielectric Constant 4.3

@Frequency 1.00e+10 Hz
4.3

@Frequency 1.00e+10 Hz
Dissipation Factor 0.016

@Frequency 1.00e+10 Hz
0.016

@Frequency 1.00e+10 Hz
Processing Properties Metric English Comments
Shelf Life 3.00 Month

@Temperature 4.44 °C
3.00 Month

@Temperature 40.0 °F
6.00 Month

@Temperature -17.8 °C
6.00 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Fabric Area Weight (g/m²) 300
Prepreg Resin Content (%) 35-45
Resin Flow (%) 8-13
325°F, 15psi