Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 393 MPa @Thickness 12.7 mm, Temperature 149 °C |
57000 psi @Thickness 0.500 in, Temperature 300 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Yield | 393 MPa @Strain 0.200 %, Thickness 12.7 mm |
57000 psi @Strain 0.200 %, Thickness 0.500 in |
|
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 393 MPa @Thickness 3.17 mm, Temperature 20.0 °C |
57000 psi @Thickness 0.125 in, Temperature 68.0 °F |
0.2% offset |
Haynes Hastelloy® C-2000® alloy, flat products Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |
|||
Tensile Strength, Yield | 393 MPa @Temperature 24.0 °C |
57000 psi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 120 Glass Fabric Hexcel designation: 120-38"-F155; Fiber: 450-1/2Information provided by HexCel |
|||
Tensile Strength, Yield | 393 MPa @Temperature 93.0 °C |
57000 psi @Temperature 199 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric Information provided by HexCel |
|||
Tensile Strength, Yield | 393 MPa @Temperature -54.0 °C |
57000 psi @Temperature -65.2 °F |
Dry |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |
|||
Tensile Strength, Yield | 393 MPa @Strain 0.200 % |
57000 psi @Strain 0.200 % |
Typical for Plate, Annealed, 0.0375" |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Yield | 393 MPa @Strain 0.200 % |
57000 psi @Strain 0.200 % |
0% Cold Work |
AK Steel NITRONIC® 30 Austenitic Stainless Steel AK Steel NITRONIC 30 Stainless Steel offers significantly higher strength than Type 304 and potential for applications requiring good resistance to aqueous and atmospheric corrosion resistance combi.. |
|||
Tensile Strength, Yield | 393 MPa @Thickness 6.35 mm, Temperature 20.0 °C |
57000 psi @Thickness 0.250 in, Temperature 68.0 °F |
0.2% offset |
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |