Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 380 MPa @Strain 1.00 % |
55100 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 1.00 % |
55100 psi @Strain 1.00 % |
Outokumpu Typical,Hot Rolled Plate (Quarto); EN 10002-1 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 % |
55100 psi @Strain 0.200 % |
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 %, Temperature -80.0 °C |
55100 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 %, Temperature -80.0 °C |
55100 psi @Strain 0.200 %, Temperature -112 °F |
EN min.; EN 10002-5 |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 %, Temperature 250 °C |
55100 psi @Strain 0.200 %, Temperature 482 °F |
EN min.; EN 10002-5 |
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Tensile Strength, Yield | >= 380 MPa @Strain 0.200 %, Thickness 15.0 - 38.1 mm |
>= 55100 psi @Strain 0.200 %, Thickness 0.591 - 1.50 in |
Tempers T651 / T652 |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 %, Thickness 127 - 152.4 mm |
55100 psi @Strain 0.200 %, Thickness 5.00 - 6.000 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | >= 380 MPa @Strain 0.200 %, Thickness 180 - 200 mm |
>= 55100 psi @Strain 0.200 %, Thickness 7.09 - 7.87 in |
|
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |
|||
Tensile Strength, Yield | 380 MPa @Strain 0.200 %, Temperature 100 °C |
55100 psi @Strain 0.200 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |