Polymer Property : Tensile Strength, Yield = 29.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.4 MPa

@Strain 5.00 %
4270 psi

@Strain 5.00 %
ASTM D638
SK Chemicals SKYPEL G182D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 29.4 MPa

@Strain 10.0 %
4270 psi

@Strain 10.0 %
ASTM D638
SK Chemicals SKYPEL G172D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Yield 29.4 MPa

@Strain 1.00 %
4270 psi

@Strain 1.00 %
ASTM D95
Daelim H&L Plavis MS Aromatic Polyimide, 15% MoS2 Filled, Machined Parts
Available in vacuum or non-lubrication condition, very high abrasion resistance and low friction coefficient propertyInformation provided by Daelim H&L
Tensile Strength, Yield 29.4 MPa

@Strain 300 %
4270 psi

@Strain 300 %
ASTM D412
SK Chemicals SKYTHANE® 395A S series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..