SK Chemicals SKYPEL G172D General Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester, TP
Manufacturer SK Chemicals
Trade Name SKYPEL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYPEL G172D General Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.017 cm/cm
0.017 in/in
ASTM D955
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength, Ultimate 46.1 MPa
6680 psi
ASTM D638
Tensile Strength, Yield 22.6 MPa

@Strain 5.00 %
3270 psi

@Strain 5.00 %
ASTM D638
29.4 MPa

@Strain 10.0 %
4270 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 420 %
420 %
ASTM D638
Flexural Modulus 0.539 GPa
78.2 ksi
ASTM D790
Izod Impact, Notched 1.18 J/cm
2.20 ft-lb/in
ASTM D256
Tear Strength 205 kN/m
1170 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 218 °C
424 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D648