Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 170 MPa @Strain 1.00 %, Temperature 400 °C |
24700 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 1.00 %, Temperature 600 °C |
24700 psi @Strain 1.00 %, Temperature 1110 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 300 °C |
24700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 300 °C |
24700 psi @Strain 0.200 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 1093 °C |
24700 psi @Strain 0.200 %, Temperature 1999 °F |
Longitudinal |
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL.. |
|||
Tensile Strength, Yield | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
|
Crucible Compaction Metals Rene Supersolvus Rene 95 Nickel Based Superalloy Supersolvus P/M Rene 95 is designed to provide even higher temperature creep resistance and stress rupture strength than subsolvus Rene 95. Chemistry is not modified. These properties are obtained.. |
|||
Tensile Strength, Yield | 170 MPa @Temperature 23.0 °C |
24700 psi @Temperature 73.4 °F |
50 mm/min; ISO 527-1/-2 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Tensile Strength, Yield | 170 MPa @Temperature 649 °C |
24700 psi @Temperature 1200 °F |
ASTM E8 |
ATI Allegheny Ludlum 309S Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Tensile Strength, Yield | 170 MPa @Strain 0.200 %, Temperature 22.2 °C |
24700 psi @Strain 0.200 %, Temperature 72.0 °F |
Typical |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |