Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 22000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 152 MPa

@Strain 1.00 %,
Temperature 500 °C
22000 psi

@Strain 1.00 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Tensile Strength, Yield 152 MPa

@Thickness 1.57 mm
22000 psi

@Thickness 0.0620 in
LW; ASTM D638
Industrial Laminates/Norplex NP843 Paper Base Laminate
Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through..
Tensile Strength, Yield 152 MPa

@Strain 0.200 %,
Temperature 760 °C
22000 psi

@Strain 0.200 %,
Temperature 1400 °F
Haynes 75 Nickel Alloy Sheet, Annealed at 1925°F (1050°C)
Haynes alloy 75 is a solution-strengthened nickel-chromium alloy with moderate strength to 1200°F (650°C). It is principally used in low stress elevated temperature applications requiring reas..
Tensile Strength, Yield 152 MPa

@Strain 0.200 %,
Temperature 371 °C
22000 psi

@Strain 0.200 %,
Temperature 700 °F
AK Steel 409 ULTRA FORM® Stainless Steel
AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and ..
Tensile Strength, Yield 152 MPa

@Temperature 649 °C
22000 psi

@Temperature 1200 °F
ASTM E8
ATI Allegheny Ludlum 309 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..
Tensile Strength, Yield 152 MPa

@Temperature 288 °C
22000 psi

@Temperature 550 °F
Longitudinal
ATI Wah Chang Zirconium Alloy Zircaloy-4
Zirconium resists corrosive attack in most organic and mineral acids, strong alkalis, and some molten salts. A tightly adherent and protective oxide film protects the metal-oxide interface to provid..
Copyright © lookpolymers.com All Rights Reserved