Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 190 MPa @Strain 1.00 %, Temperature 400 °C |
27600 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 200 °C |
27600 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 400 °C |
27600 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 200 °C |
27600 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4310 Cr-Ni Austenitic Stainless Steel Cold work hardening steel suitable for manufacture of springs operating in corrosive conditions.Available hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and ro.. |
|||
Tensile Strength, Yield | 190 MPa @Strain 0.200 %, Temperature 200 °C |
27600 psi @Strain 0.200 %, Temperature 392 °F |
EN min.; EN 10002-5 |
Outokumpu 4529 Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Tensile Strength, Yield | 190 MPa @Temperature 177 °C |
27600 psi @Temperature 351 °F |
Wet |
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195Information provided by HexCel |