Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 125 MPa @Strain 1.00 %, Temperature 400 °C |
18100 psi @Strain 1.00 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
Tensile Strength, Yield | 125 MPa @Strain 0.200 %, Temperature 400 °C |
18100 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 4550 Austenitic Stainless Steel Good corrosion resistance and weldable. Resistant to sensitization.Applications: Welded screensFurnace beltsCatalytic converter meshAvailable in hot rolled plate (Quarto) and rod forms. |
|||
Tensile Strength, Yield | 125 MPa @Temperature 150 °C |
18100 psi @Temperature 302 °F |
ASTM D638 |
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in .. |
|||
Tensile Strength, Yield | >= 125 MPa @Strain 0.200 %, Thickness 5.00 - 6.30 mm |
>= 18100 psi @Strain 0.200 %, Thickness 0.197 - 0.248 in |
Temper H111; Standard EN 485-2 |
Constellium PLAN 5083 Aluminum Rolled Plate Rolled plates in 5083 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5083 PLAN is mainly used for low stressed mechanical components, manufactured by intensive m.. |
|||
Tensile Strength, Yield | 125 MPa @Strain 0.200 %, Thickness 120 - 150 mm |
18100 psi @Strain 0.200 %, Thickness 4.72 - 5.91 in |
Typical Strength |
Constellium ALPLAN® 5083 Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 5083 precision plates exhibit good dimensional stability. Their low internal stresses reduces the effects of plate deformation during machining, thus saving on extra operations such as roug.. |
|||
Tensile Strength, Yield | 125 MPa @Temperature 40.0 °C |
18100 psi @Temperature 104 °F |
ISO 527 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Strength, Yield | 125 MPa @Strain 0.200 %, Temperature 400 °C |
18100 psi @Strain 0.200 %, Temperature 752 °F |
EN min.; EN 10002-5 |
Outokumpu 904L High Performance Austenitic Stainless Steel Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar.. |