Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 103 MPa @Thickness 3.17 mm |
15000 psi @Thickness 0.125 in |
LW |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Tensile Strength, Yield | 103 MPa @Thickness 1.57 mm |
15000 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP843 Paper Base Laminate Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP843 has conductive surfaces only, as compared to NP842, which is conductive through.. |